Reinforcing bars

Thermo-mechanically treated reinforcing die-rolled section bars At800 class

Range:
Ø  10, 12, 14 mm
Steel grade:
25G2S
Standard:
GOST 10884-94 (RB excluded), GOST 34028-2016

Strength class of reinforcing steel Nominal diameter, mm Electric heating temperature,° C Mechanical properties Bending test on the cold, °С The diameter of the mandrel (d - nominal diameter of the rod)
Tensile strength δB, N/mm2 Conventional physical and yield strength
δ0,2t) N/mm2
Relative elongation, %
δ5 δp
no less
At400 6-40   550 440 16   90 3d
At500 6-40 600 500 14 90
At600 10-40 400 800 600 12 4 45 5d
At800 10—32* 400 1000 800 8 2 45
At1000 10-32 450 1250 1000 7 2 45
At1200 10—32 450 1450 1200 6 2 45

* For reinforcing steel class At800K diameter 18-32 mm.

Remarks:

1. For rebar At600S class may decrease the ultimate tensile strength of 50 N/mm2below norms established table, with increasing elongation δ5 2% (abs.) And uniform elongation δp 1% (abs.).
2. Reinforcing steel grades at400s, at500s and at600 in rods tensile strength should not exceed the values given in the table, more than 200 n/mm 2.
3. For the reinforcing steel strength class At1200 delivery state may decrease proof stress up to 1150 N/mm2.
4. When testing reinforcing steel grades At800 strength At1000 and At1200 immediately after rolling is allowed to decrease the ductility indices 1% (abs).

In bundles, weight 5 tons max., with banding by wire rod 6,5 mm in 6 places min. equally distributed over bundle. Each bundle is provided with 2 steel straps for multiple lifting.